Effect of Build Orientation and Feature Geometry on Dimensional Deviations in Resin-Based (SLA) 3D Printing

Authors

  • Ece Ayaz Kocaeli University
  • Gökşan Şan ARaymond Türkiye
  • Alp Eren Şahin ARaymond Türkiye

Keywords:

SLA (stereolithography), DLP, Resin 3D printing, , Shrinkage, Dimensional deviation, Build orientation, Pixelisation, Additive manufacturing, Photopolymer resin

Abstract

This study investigates the dimensional deviations and shrinkage behaviour of parts produced on a resin-based (DLP-type) 3D printer without any dimensional compensation (offset), as is common practice in prototyping and testing. A single test artefact containing circular and square features with and without holes, in four sizes and in four regions (sections) with different wall-thickness conditions, was designed in Creo, sliced in Chitubox (50 µm layers, 2.1 s exposure) and printed from a single lot of Loctite 3D Pro 417 resin at three build orientations (0°, 22.5° and 45°), with three replicate builds per orientation. After identical cleaning and post-curing, outer dimensions, hole dimensions, inter-feature gaps, ovality and axis offset were measured 72 h after curing on a Mitutoyo Quick Vision Apex vision measuring system, with diameters evaluated as average (least-squares) sizes in accordance with ISO 14405-1, and expressed as deviations from nominal (measured minus nominal). The smallest dimensional and geometric deviations were obtained at 0°, where the part is fully restrained by the build plate: outer contours were oversized by roughly 0.05–0.20 mm while holes were undersized (about −0.16 mm for the square holes of Section 1), a pattern consistent with an edge-growth (light-bleed/pixel-discretisation) effect of the order of one projector pixel (≈52 µm) superimposed on a near-zero net shrinkage. At inclined orientations the edge-growth signature disappeared and a common positive offset of about 0.1–0.2 mm appeared on both internal and external features; hole deviations were the most orientation-sensitive quantity and reached +0.20 mm (circular) and +0.19 mm (square) at 45°, with a pronounced X/Y anisotropy (Y up to +0.23 mm). The nominal 1 mm gaps between features were undersized at every position at 0° and 22.5°, indicating genuine material closure. The results show that build orientation, feature geometry, feature size and position on the build plate must be considered together, and that a 0° orientation combined with a small negative XY compensation is the most favourable strategy for hole-critical features. Indicative first-order compensation values are derived from the measurements.

Downloads

Download data is not yet available.

Author Biographies

Ece Ayaz, Kocaeli University

Department of Mechanical Engineering, Kocaeli, Türkiye

Gökşan Şan, ARaymond Türkiye

Design Center,  Kocaeli, Türkiye

Alp Eren Şahin, ARaymond Türkiye

Design Center, Kocaeli, Türkiye

Downloads

Published

2026-10-07

How to Cite

Ayaz, E., Şan, G., & Şahin, A. E. (2026). Effect of Build Orientation and Feature Geometry on Dimensional Deviations in Resin-Based (SLA) 3D Printing. International Journal of Advanced Natural Sciences and Engineering Researches, 10(10), 177–197. Retrieved from https://as-proceeding.com/index.php/ijanser/article/view/3280

Issue

Section

Articles